Fire Performance of FRP:

پدید آورنده
Mousavi, Seyed Mohammad Sadegh Arshia

موضوع
Cold,Load,Mechanical properties,Parking facilities,Polymers,Software

رده

کتابخانه
Center and Library of Islamic Studies in European Languages

محل استقرار
استان: Qom ـ شهر: Qom

Center and Library of Islamic Studies in European Languages

تماس با کتابخانه : 32910706-025

NATIONAL BIBLIOGRAPHY NUMBER

Number
TLpq2525583076

LANGUAGE OF THE ITEM

.Language of Text, Soundtrack etc
انگلیسی

TITLE AND STATEMENT OF RESPONSIBILITY

Title Proper
Fire Performance of FRP:
General Material Designation
[Thesis]
First Statement of Responsibility
Mousavi, Seyed Mohammad Sadegh Arshia
Title Proper by Another Author
Bond of GFRP Bars to Concrete and FRP Strengthened Columns
Subsequent Statement of Responsibility
Green, Mark F.

.PUBLICATION, DISTRIBUTION, ETC

Name of Publisher, Distributor, etc.
Queen's University (Canada)
Date of Publication, Distribution, etc.
2020

PHYSICAL DESCRIPTION

Specific Material Designation and Extent of Item
109

DISSERTATION (THESIS) NOTE

Dissertation or thesis details and type of degree
M.A.Sc.
Body granting the degree
Queen's University (Canada)
Text preceding or following the note
2020

SUMMARY OR ABSTRACT

Text of Note
Standard pullout tests (e.g. 200 mm cubes) with a short embedment length have shown a significant reduction (80% loss at 200 °C) in the bond strength of GFRP bars at high temperatures. More detailed bond behaviour of glass fibre reinforced polymer (GFRP) reinforcing bars has been examined in this study. This study adopted a modified pullout test method in which pullout specimens consisting of GFRP bars embedded in 350 mm (22db) long concrete cylinders are tested at high temperatures. The tests examined the bond degradation under different temperature distributions (i.e. uniform and gradient). The results were compared with the previous pullout tests with 68 mm (4db) embedment length and showed that the pullout capacity of GFRP bars in this test were 3.3, 4, and 2 times higher at 115, 135 and 300 °C, respectively. The results proved the effectiveness of longer embedment length particularly at temperatures below 200 °C. Pullout tests with temperature gradients simulated the bond behaviour of GFRP bars at the unexposed end zones of GFRP reinforced concrete beams or slabs. The results showed that the tensile force in GFRP bars gradually transferred to the lower temperature zones as the heated parts of the bar lost bond with concrete. The results showed that the concentrated forces over a short length of GFRP can trigger concrete splitting and loss of bond even if the GFRP bars still maintain bond with concrete. Providing thicker concrete cover at the end zones of GFRP reinforced members is recommended to enhance fire resistance. Also, a series of approximate and simple numerical models including heat and structural analysis were developed to study the effects of high temperatures on two FRP-wrapped and insulated reinforced concrete columns tested by the National Research Council (NRC) of Canada. The results of finite element models showed less than 5% difference with the experimental results.

TOPICAL NAME USED AS SUBJECT

Cold
Load
Mechanical properties
Parking facilities
Polymers
Software

PERSONAL NAME - PRIMARY RESPONSIBILITY

Green, Mark F.
Mousavi, Seyed Mohammad Sadegh Arshia

ELECTRONIC LOCATION AND ACCESS

Electronic name
 مطالعه متن کتاب 

p

[Thesis]
276903

a
Y

Proposal/Bug Report

Warning! Enter The Information Carefully
Send Cancel
This website is managed by Dar Al-Hadith Scientific-Cultural Institute and Computer Research Center of Islamic Sciences (also known as Noor)
Libraries are responsible for the validity of information, and the spiritual rights of information are reserved for them
Best Searcher - The 5th Digital Media Festival